MP35N nickel bar manufacture, MP35N nickel wire rod Alloy MP35N® (AMS 5844/AMS 5845/ NACE MR0175)
▪ UNS R30035
▪ AMS 5758 - MP35N® VIM-VAR Bar
▪ Solution heat treated @1900-1925°F for 4 to 8 hours
▪ AMS 5844 - MP35N® VIM-VAR Bar
▪ Solution heat treated @1900-1925°F for 4 to 8 hours and Work Strengthened
▪ AMS 5845 - MP35N® VIM-VAR Bar
▪ Solution heat treated @ 1900-1925°F for 4 to 8 hours, Work Strengthened & Aged @ 1000-1200°F for 4 hours
▪ NACE MR0175
▪ ASTM F-562 - Surgical Implant Applications
▪ BS 7252-6 Surgical Implant Applications
▪ ISO 5832-6 Surgical Implant Applications
MP35N is extremely suitable in environments where a high combination of strength, high modulus values, and good corrosion resistance are required. Some examples of these types of applications, include:
▪ Medical devices
▪ Dental products
▪ Marine engineering
In addition, MP352 can be used to manufacture fasteners, springs, non-magnetic components and instrumentation in medical, seawater, oil and gas wells, chemical and food processing environments.
Weight % | Ni | Co | Cr | Mo | Ti | Fe | Si | Mn | P | B | S | C |
MP35N | 33-37 | Bal | 19-21 | 9-10.5 | 1 max | 1 max | 0.15 max | 0.15 max | 0.015 max | 0.010 max | 0.010 max | 0.03 max |
Material | Condition | Ultimate Tensile Strength ksi | 0.2 % Yield Strength ksi | Elongation % | Reduction of Area % | Hardness HRC |
MP35N AMS 5844 |
Solution Heat Treated and Work Strengthened | 255 | 225 | 12 | 50 | 45 |
MP35N AMS 5845 |
Solution Heat Treated and Work Strengthened and Aged | 260 | 230 | 8 | 35 | 38 min |